Nominal or standard size, inches | Nominal dimensions, inches | Calculated values (based on nominal dimensions) |
Outside diameter | Inside diameter | Wall thickness | Cross sectional area of bore, sq. inches | Weight of tube only, pounds per linear ft. | Weight of tube & water, pounds per linear ft. | Volume of tube, per linear ft. |
Cu ft. | Gal. |
11⁄4 |
1.375 |
1.295 |
.040 |
1.32 |
.650 |
1.22 |
.00917 |
.0686 |
11⁄2 |
1.625 |
1.541 |
.042 |
1.87 |
.809 |
1.62 |
.0130 |
.0971 |
2 |
2.125 |
2.041 |
.042 |
3.27 |
1.07 |
2.48 |
.0227 |
.170 |
3 |
3.125 |
3.030 |
.045 |
7.21 |
1.69 |
4.81 |
.0501 |
.375 |
4 |
4.125 |
4.009 |
.058 |
11.6 |
2.87 |
7.88 |
.0806 |
.603 |
5 |
5.125 |
4.981 |
.072 |
19.5 |
4.43 |
12.9 |
.135 |
1.01 |
6 |
6.125 |
5.959 |
.083 |
27.9 |
6.10 |
18.2 |
.194 |
1.45 |
8 |
8.125 |
7.907 |
.109 |
49.1 |
10.6 |
31.8 |
.341 |
2.55 |