level2b
Table 14.2b. Dimensions and Physical Characteristics of Copper Tube: Type L
Nominal or standard size, inches | Nominal dimensions, inches | Calculated values (based on nominal dimensions) |
Outside diameter | Inside diameter | Wall thickness | Cross sectional area of bore, sq. inches | Weight of tube only, pounds per linear ft. | Weight of tube & water, pounds per linear ft. | Volume of tube, per linear ft. |
Cu ft. | Gal. |
1⁄4 |
.375 |
.315 |
.030 |
.078 |
.126 |
.160 |
.00054 |
.00405 |
3⁄8 |
.500 |
.430 |
.035 |
.145 |
.198 |
.261 |
.00101 |
.00753 |
1⁄2 |
.625 |
.545 |
.040 |
.233 |
.285 |
.386 |
.00162 |
.0121 |
5⁄8 |
.750 |
.666 |
.042 |
.348 |
.362 |
.506 |
.00232 |
.0174 |
3⁄4 |
.875 |
.785 |
.045 |
.484 |
.455 |
.664 |
.00336 |
.0251 |
1 |
1.125 |
1.025 |
.050 |
.825 |
.655 |
1.01 |
.00573 |
.0429 |
11⁄4 |
1.375 |
1.265 |
.055 |
1.26 |
.884 |
1.43 |
.00875 |
.0655 |
11⁄2 |
1.625 |
1.505 |
.060 |
1.78 |
1.14 |
1.91 |
.0124 |
.0925 |
2 |
2.125 |
1.985 |
.070 |
3.09 |
1.75 |
3.09 |
.0215 |
.161 |
21⁄2 |
2.625 |
2.465 |
.080 |
4.77 |
2.48 |
4.54 |
.0331 |
.248 |
3 |
3.125 |
2.945 |
.090 |
6.81 |
3.33 |
6.27 |
.0473 |
.354 |
31⁄2 |
3.625 |
3.425 |
.100 |
9.21 |
4.29 |
8.27 |
.0640 |
.478 |
4 |
4.125 |
3.905 |
.110 |
12.0 |
5.38 |
10.1 |
.0764 |
.571 |
5 |
5.125 |
4.875 |
.125 |
18.7 |
7.61 |
15.7 |
.130 |
.971 |
6 |
6.125 |
5.845 |
.140 |
26.8 |
10.2 |
21.8 |
.186 |
1.39 |
8 |
8.125 |
7.725 |
.200 |
46.9 |
19.3 |
39.6 |
.326 |
2.44 |
10 |
10.125 |
9.625 |
.250 |
72.8 |
30.1 |
61.6 |
.506 |
3.78 |
12 |
12.125 |
11.565 |
.280 |
105 |
40.4 |
85.8 |
.729 |
5.45 |