level2b
Table 14.2a. Dimensions and Physical Characteristics of Copper Tube: Type K
Nominal or standard size, inches | Nominal dimensions, inches | Calculated values (based on nominal dimensions) |
Outside diameter | Inside diameter | Wall thickness | Cross sectional area of bore, sq. inches | Weight of tube only, pounds per linear ft. | Weight of tube & water, pounds per linear ft. | Volume of tube, per linear ft. |
Cu ft. | Gal. |
1⁄4 |
.375 |
.305 |
.035 |
.073 |
.145 |
.177 |
.00051 |
.00379 |
3⁄8 |
.500 |
.402 |
.049 |
.127 |
.269 |
.324 |
.00088 |
.00660 |
1⁄2 |
.625 |
.527 |
.049 |
.218 |
.344 |
.438 |
.00151 |
.0113 |
5⁄8 |
.750 |
.652 |
.049 |
.334 |
.418 |
.562 |
.00232 |
.0174 |
3⁄4 |
.875 |
.745 |
.065 |
.436 |
.641 |
.829 |
.00303 |
.0227 |
1 |
1.125 |
.995 |
.065 |
.778 |
.839 |
1.18 |
.00540 |
.0404 |
11⁄4 |
1.375 |
1.245 |
.065 |
1.22 |
1.04 |
1.57 |
.00847 |
.0634 |
11⁄2 |
1.625 |
1.481 |
.072 |
1.72 |
1.36 |
2.10 |
.0119 |
.0894 |
2 |
2.125 |
1.959 |
.083 |
3.01 |
2.06 |
3.36 |
.0209 |
.156 |
21⁄2 |
2.625 |
2.435 |
.095 |
4.66 |
2.93 |
4.94 |
.0324 |
.242 |
3 |
3.125 |
2.907 |
.109 |
6.64 |
4.00 |
6.87 |
.0461 |
.345 |
31⁄2 |
3.625 |
3.385 |
.120 |
9.00 |
5.12 |
9.01 |
.0625 |
.468 |
4 |
4.125 |
3.857 |
.134 |
11.7 |
6.51 |
11.6 |
.0813 |
.608 |
5 |
5.125 |
4.805 |
.160 |
18.1 |
9.67 |
17.5 |
.126 |
.940 |
6 |
6.125 |
5.741 |
.192 |
25.9 |
13.9 |
25.1 |
.180 |
1.35 |
8 |
8.125 |
7.583 |
.271 |
45.2 |
25.9 |
45.4 |
.314 |
2.35 |
10 |
10.125 |
9.449 |
.338 |
70.1 |
40.3 |
70.6 |
.487 |
3.64 |
12 |
12.125 |
11.315 |
.405 |
101 |
57.8 |
101 |
.701 |
5.25 |