Ceridian Corporate Headquarters

Bloomington, Minnesota

New Construction

Architect

Hammel, Green and Abrahamson, Inc.
Minneapolis, Minnesota

Copper System: Laminated copper facing on a thermoplastic core on a stainless steel subgirt system

For this curtain wall system a composite copper panel was used. This panel offers strength and a dead flat surface preventing "oil canning". Oil canning is a term used to describe the waviness that is common with sheet metal roof and wall systems.

Architectural Category: Exotic or Unusual Applications